Made some slabs for my Green River blades. They are machined hard anodized aluminum. They look great (bad pics), but might be cold and slick outdoors.
I put a layer of epoxy between the slabs and the full tang in the hopes of preventing a reaction between the metals. Comments on whether that will work? What is that reaction again?